Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.800 - 1.40 g/cc | 0.0289 - 0.0506 lb/in³ | |
Solvay Chemicals (CsAlF4) Cesium Tetrafluoroaluminate Flux for brazing aluminum. Particularly suitable for flame brazing of magnesium-containing aluminum alloys.HS No.: 38109090 /CAS-No.: 39211-00-2Uses: Automotive Sector, Commercial & Residential Ai.. |
|||
Bulk Density | 1.30 - 1.40 g/cc | 0.0470 - 0.0506 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE MW Refractory Insulating Castable Description: Golite MW (medium weight) is composed of a light weight refractory aggregate plus several additives to improve the mechanical properties.Remarks: These values apply to cast products. Al.. |