Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9212 E Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9216 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.20 - 1.35 g/cc | 0.0434 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9510 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9612 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9620 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9622 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.20 - 1.35 g/cc | 0.0434 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9634 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9816 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.25 - 1.35 g/cc | 0.0452 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9923 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |