Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.00 - 1.10 g/cc | 0.0361 - 0.0397 lb/in³ | |
Nabaltec GRANALOX® NM 9922 I Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 0.900 - 1.10 g/cc | 0.0325 - 0.0397 lb/in³ | |
Nabaltec NABALOX® NO 102 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.900 - 1.10 g/cc | 0.0325 - 0.0397 lb/in³ | |
Nabaltec NABALOX® NO 103 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.900 - 1.10 g/cc | 0.0325 - 0.0397 lb/in³ | |
Magyar Aluminum ALO-B15 Alumina Calcined Alumina; Minimum 5% alpha-Al2O3. |
|||
Bulk Density | 0.800 - 1.10 g/cc | 0.0289 - 0.0397 lb/in³ | |
Magyar Aluminum ALO-DFC Alumina Alumina for Polishing |
|||
Bulk Density | 0.900 - 1.10 g/cc | 0.0325 - 0.0397 lb/in³ | |
Magyar Aluminum ALO-P90 Alumina Alumina for Polishing |
|||
Bulk Density | 1.00 - 1.10 g/cc | 0.0361 - 0.0397 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 1.2.4. Mix Refractory Insulating Castable Description: This lightweight castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Remarks: Th.. |
|||
Bulk Density | 1.00 - 1.10 g/cc | 0.0361 - 0.0397 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va.. |