Polymer Property : Bulk Density = 0.0343 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.850 - 0.950 g/cc
0.0307 - 0.0343 lb/in³
PEPL-10-W-67
Pearl Engineering PEPLPET B-109JS PET Sheet Grade
Used mainly for 5 to 20 liter mineral water containers
Bulk Density 0.850 - 0.950 g/cc
0.0307 - 0.0343 lb/in³
PEPL-10-W-67
Pearl Engineering PEPLPET B-113C PET Sheet Grade
Used mainly for box strapping.
Bulk Density 0.700 - 0.950 g/cc
0.0253 - 0.0343 lb/in³
Magyar Aluminum ALO-P54 Alumina
Alumina for Polishing
Bulk Density 0.850 - 0.950 g/cc
0.0307 - 0.0343 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable
Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati..
Bulk Density 0.850 - 0.950 g/cc
0.0307 - 0.0343 lb/in³
DIN 53466
Stanelco Bioplast® Wrap 100 Biodegradable Plastic
Bioplast Wrap 100 is a plasticiser-free thermoplastic material which allows the production of films with coated paper-like properties. Wrap 100 is an excellent, eco-friendly alternative to laminated..
Bulk Density 0.750 - 0.950 g/cc
0.0271 - 0.0343 lb/in³
Powder Density; ISO 60
Vyncolit 3640 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..