Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 115 TC Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 115-25 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 115-71 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Nabaltec NABALOX® NO 325 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-105C PET Bottle Grade A co-polymer used for soft drinks and other applications. |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-103C PET Bottle Grade A co-polymer used for mineral water bottles |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
Taiwan PU Corporation MOCA Polyurethane Resin Curing Agent MOCA [4,4' - Methylene bis-(ortho-chloroaniline)] is used as a PU curing agent. The chlorine atoms on benzene ring can slow down the activity of the NH2 group, so as to extend the pot life while ca.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
Solvay Chemicals NOCOLOK® Flux Drystatic Potassium Fluoroaluminate Flux using electrostatic/dry powder coating. Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & .. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
Solvay Chemicals NOCOLOK® Li Flux Drystatic Flux for aluminum brazing with further reduced residue solubility and improved corrosion characteristics and using electrostatic/dry powder coating.HS No.: 38109090 /CAS-No.: 60304-36-1 and 13821-.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BB7755 Specially Formulated PET Resin Description: SKYPET-BB7755 is a specially formulated PET resin for PET bottles especially for hot-fill application. SKYPET-BB7755 provides excellent processability in injection molding and blow mol.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BL8050 Specially Formulated PET Copolymer Resin SKYPET-BL8050 is a specially formulated PET copolymer resin for PET bottles and extruded sheet. SKYPET-BL8050 provides excellent processability in injection molding and blow molding processes, offe.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BR8040 Low Content CHDM Modified Copolyester Resin Description: SKYPET-BR8040 is a low content CHDM modified copolyester resin for large sized-mineral water bottles and extruded sheet. SKYPET-BR8040 has sufficiently low crystallization rate for lar.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® XT8050 Specially Formulated PET Copolymer Resin Description: SKYPET-XT8050 is a fast reheat grade of SKYPET, specially formulated for high productivity in the blowing process. SKYPET-XT8050 provides excellent processability in injection molding .. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BB8055 Specially Formulated PET Resin Description: SKYPET-BB8055 is a specially formulated PET resin for PET bottles especially for hot-fill application. SKYPET-BB8055 provides excellent processability in injection molding and blow mol.. |
|||
Bulk Density | 0.820 - 0.900 g/cc | 0.0296 - 0.0325 lb/in³ | |
SK Chemicals SKYPET® BL8450 Specially Formulated PET Copolymer Resin Description: SKYPET-BL8450 is a specially formulated PET copolymer resin for PET bottles and extruded sheet. SKYPET-BL8450 provides excellent processability in injection molding and blow molding pr.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic .. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4406 G3 Uncolored Q717 PBT Information provided by BASF |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4520 High Speed PBT Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4560 PBT Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF |
|||
Bulk Density | 0.650 - 0.900 g/cc | 0.0235 - 0.0325 lb/in³ | |
BASF Ultraform® N2720 M210 POM Description: Is a POM, product with increased stiffness and strength as well as good wear characteristics, used, for instance, for sliding chains and conveyor systems.Information provided by BASF |
|||
Bulk Density | 0.650 - 0.900 g/cc | 0.0235 - 0.0325 lb/in³ | |
BASF Ultraform® N2770 K POM Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
Addcomp ADD-VANCE® BA 401 Blowing agent Fields of application: Foamed products of Polyolefin and other polymers.Examples: Extruded sheets and foams in general as well as injection molded parts that require a foamed core.Mode of action and.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4500 BK 00110 PBT Information provided by BASF |
|||
Bulk Density | 0.750 - 0.900 g/cc | 0.0271 - 0.0325 lb/in³ | Powder Density; ISO 60 |
Vyncolit 3520 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4040 G6 30% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 30% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled BK 15045 PBT Description: Easy flowing injection molding grade with 15 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg timer dials, toggles, knobs, parts for thermostats, oven-door .. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, .. |