Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Nabaltec NABALOX® NO 313 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Magyar Aluminum ALO-P54-04 Alumina Alumina for Polishing |
|||
Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
LG Chemical SAP Super Absorbent Polymer Features: Super Absorbent Polymer absorbs pure water at several-hundred times of its dry weight. They are used extensively as the raw materials for various industries in baby diaper, feminine hygien.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
Sharadaa Ceramics CFI Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
Solvay RHODICARE CFT Surfactant Description: Rhodicare® CFT is Cellulase-free clear grade of Xanthan Gum, it is recommended when associated with cellulose-based polymers. Approved for Ecocert. It is excellent anionic bio-polyme.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
Solvay RHODICARE T Surfactant Description: Rhodicare® T is high purity grade specifically designed for thickening and suspension in clear formulations. It has high electrolyte stability over a wide range of pH and fast hydrat.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
Solvay RHODOPOL® T Surfactant Description: Transparent grade xanthan gum. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent.Identification: XANTHAN GUMCAS: 11138 – 66 – 2Available.. |
|||
Bulk Density | 0.650 - 0.800 g/cc | 0.0235 - 0.0289 lb/in³ | Powder Density; ISO 60 |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
Bulk Density | 0.650 - 0.800 g/cc | 0.0235 - 0.0289 lb/in³ | |
Addcomp ADD-VANCE® DS 785 Desiccant masterbatch in PP carrier Fields of application: Highly concentrated desiccant masterbatch for HDPE and PP.Examples: Elimination of moisture from (recycle) polymers in moisture sensitive applications.Mode of action and advan.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® 1C PA6/66 (Dry) Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Informa.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Conditioned) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry) Description: 50% glass fiber reinforced injection molding grade with optimized heat ageing performance for industrial articles having very high rigidity.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® A4H PA66 (Dry) Description: Highly heat aging resistant, medium-viscosity injection-molding grade for highly stressed parts such as bearing cages, gearwheels, spool bodies and chain drive tensioners.Information pr.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3WG6 HP BK 23210 30% Glass Filled PA6 (Dry) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade with enhances flowability used e.g. for automobile manifold.Information provided by BASF |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |
|||
Bulk Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry) Description: 25% glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used fo.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® BG40GM45 HS BK 00130 20/25 % Glass/Mineral Filled PA6 (Dry) Description: Ultramid® BG40GM45 HS BK-130 is a pigmented black, heat stabilized, 45 % glass and mineral fiber reinforced polyamide 6 injection molding compound. It possesses a balance of engineerin.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® Seal-Fit PA6/66 (Conditioned) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |