Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EA3350 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Medical containersBlends with clear SB-copolymersClam-shell containersBi-axially oriented sheetFeatures:High molecular weight homopolymerHigh Vicat softeni.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips MC3200 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Medical partsConsumer containers, vials, jars, etc.Clock lensesAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat softening tempera.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips MC3600 Crystal Polystyrene
(discontinued **) General purpose crystal polystyrene.Applications:HousewaresConsumer containers, vials, jars, etc.Disposable cutleryInjection molded drink cupsFeatures:Easy filling of thin-walled partsExceptional mo.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EB6025 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Cosmetic packagingShower surroundsPoint of purchase displaysThin-wall injection molding and thermoformingFeatures:Smooth, glossy surface finishGo.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EC6400 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EC6755 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Containers and lidsPackaging for foods such as yot, sour cream, delicatessen salads and gravyCold temperature packagingPortion dairy containersFe.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips MA5350 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Floppy diskettesDurable household applicationsThin to medium parts that require a combination of high gloss and good toughnessFeatures:Low coeffi.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips MD6800 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Displays and retail product shelvingDurable household applicationsThin to medium thickness parts that require a combination of high flow and good.. |
|||
Bulk Density | 0.561 - 0.673 g/cc | 0.0203 - 0.0243 lb/in³ | Loose |
KaMin KaMin® 611 Kaolin Clay - Waterwashed Naturally delaminated clay for use in water-based paints and coatings.Industry: Paint & CoatingsUses: Industrial Coatings, E-Coat, PrimerInformation provided by KaMin LLC. |
|||
Bulk Density | 0.561 - 0.673 g/cc | 0.0203 - 0.0243 lb/in³ | Loose |
KaMin KaMin® 90B Kaolin Clay - Waterwashed KaMin® 90B is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90B is ideally suited for water-borne applications where high gloss, holdout and .. |
|||
Bulk Density | 0.561 - 0.673 g/cc | 0.0203 - 0.0243 lb/in³ | Loose |
KaMin Polyfil® FB Kaolin Clay - Waterwashed Water washed kaolin clays such as Polyfil® FB offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® FB is a moderate brightness wate.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EB6400 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EC6600 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Lithographic sheetPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Excellent printabilityMatte surface finishHigh hea.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips MB3150 Crystal Polystyrene High heat crystal polystyrene.Applications:Compact disc jewel boxesConsumer containers, vials, jars, etc.Desk organizersAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat sof.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips MC3650 Crystal Polystyrene General purpose crystal polystyrene.Applications:HousewaresConsumer containers, vials, jars, etc.Disposable cutleryInjection molded drink cupsFeatures:Easy filling of thin-walled partsExceptional mo.. |
|||
Bulk Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Chevron Phillips EA3025 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Foam egg cartonsFoam meat traysInsulation boardBi-axially oriented sheetFeatures:Ultra-high molecular weight homopolymerHigh Vicat softening temperatureNar.. |