Physical Properties Metric English Comments
Bulk Density 0.529 - 0.593 g/cc
0.0191 - 0.0214 lb/in³
ASTM D1895
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade
ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu..