Physical Properties Metric English Comments
Bulk Density 2.68 g/cc
0.0968 lb/in³
Chosun Refractories SBSN-AN Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.68 g/cc
0.0968 lb/in³
Chosun Refractories SSB-3 Bricks, Reaction Bonded SiC