Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | |
Nabaltec GRANALOX® NM 9620 F Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | |
Nabaltec GRANALOX® NM 9922 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | <= 1.15 g/cc | <= 0.0415 lb/in³ | |
Magyar Aluminum ALOLT 21AF Aluminum Hydroxide Ground type |
|||
Bulk Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 135 RL C Refractory Insulating Castable Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast .. |
|||
Bulk Density | 1.15 g/cc | 0.0415 lb/in³ | |
DuPont™ Nomex® 418 Paper, 8 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |