Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
Nabaltec APYRAL® 32 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ISO 60 |
FKuR Kunststoff Fibrolon® F 8530 Biodegradable Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Depending on specific customer requirements either a biodegradable polymer or a polyolefin can be used as the polymeric matrix. With the brand name of F.. |
|||
Bulk Density | 0.641 - 0.721 g/cc | 0.0231 - 0.0260 lb/in³ | |
Green Dot Terratek® SC 50 Polypropylene - Wheat Starch Biocomposite Terratek® SC 50 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 50 contains 50% wheat starch by weight, however, a range of properties can be achie.. |
|||
Bulk Density | 0.641 - 0.721 g/cc | 0.0231 - 0.0260 lb/in³ | |
Green Dot Terratek® SC 65 Polypropylene - Wheat Starch Biocomposite Terratek® SC 65 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 65 contains 65% wheat starch by weight, however, a range of properties can be achie.. |
|||
Bulk Density | 0.641 - 0.721 g/cc | 0.0231 - 0.0260 lb/in³ | Loose |
KaMin Polyfil® DLX Kaolin Clay - Delaminated Polyfil DLX is a large particle size, very high aspect ratio, delaminated clay that reduces gas and vapor permeability. It is a type of water washed clay which is processed to have a high aspect rat.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | Tap Density |
SGL Carbon Group CF 480 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D1895 |
Plenco 2311 Phenolic, Granular, Injection Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D1895 |
Plenco 4349 Phenolic, Granular, Transfer Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D1895 |
Plenco 4485 Phenolic, Granular, Injection Molded PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | Tap |
TIMCAL TIMREX® T800 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ISO 60 |
Vyncolit X7012 Glass Fiber Reinforced Novolac Phenolic Novolac resin based, glass fiber and glass beads reinforced. High mechanical strength even at high temperatures in Long Life CoolantsInformation provided by Sumitomo Bak North America, Inc. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D1895 |
Plenco 2571 Phenolic, Granular, Injection Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 6165 X Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Low.. |
|||
Bulk Density | 0.641 - 0.705 g/cc | 0.0231 - 0.0255 lb/in³ | loose |
CIMBAR CAL-BEN™ Calcium Bentonite Selectively mined calcium bentonite, specially blended and processed for general industrial use. It is tan to yellowish in color and comes in the form of a fine powder.Incorporation:Can be base exc.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
BASF Styropor® BF 422 EPS Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
BASF Styropor® BFL 222 EPS Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
BASF Styropor® BFL 322 EPS Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
BASF Styropor® BFL 422 EPS Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
BASF Styropor® BF 327 EPS Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv.. |
|||
Bulk Density | 0.640 - 0.740 g/cc | 0.0231 - 0.0267 lb/in³ | |
BASF Ultramid® B36 LNV PA6 Information provided by BASF |
|||
Bulk Density | 0.640 - 0.740 g/cc | 0.0231 - 0.0267 lb/in³ | |
BASF Ultramid® B40 L PA6 Description: Ultramid® B40 L is a lubricated polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film and monofilaments. Product supplied in 2-2.5 mm round .. |
|||
Bulk Density | 0.640 - 0.740 g/cc | 0.0231 - 0.0267 lb/in³ | |
BASF Ultramid® B40 LN PA6 Description: Ultramid® B40 LN is a polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film. Clarity and thermoformability are enhanced by the incorporation.. |
|||
Bulk Density | 0.640 - 0.740 g/cc | 0.0231 - 0.0267 lb/in³ | |
BASF Ultramid® B40 PA6 Description: Ultramid® B40 is a polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film and monofilaments. Product supplied in 2-2.5 mm round pellets.Infor.. |
|||
Bulk Density | 0.640 - 0.740 g/cc | 0.0231 - 0.0267 lb/in³ | |
BASF Ultramid® B27 SD 02 PA6 Description: Ultramid® B27 SD 02 is a polyamide 6 for the production of semi dull textile and carpet fibers. Product comes in 2-2.5 mm cylindrical pellets.Information provided by BASF |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
BASF Styropor® BF 322 EPS Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv.. |