Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Nabaltec NABALOX® NO 113 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895B |
SABIC PS 155 General Purpose Polystyrene for Foam Extrusion Product Description: General purpose Polystyrene PS 155 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and go.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895B |
SABIC PS 160 General Purpose Polystyrene for Foam Extrusion Product Description: General purpose Polystyrene PS 160 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle material having High molecular .. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | |
Raschig Group PiMC 1253 Highly flame retardant This FR PiMC grade has been developed for top coats over M1 SMC/BMC grades. Such combinations will meet Europe’s most stringent FR tests for interiors of rolling stock, such as BS 476 and Spanish E.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895B |
SABIC PS 330 High Impact Polystyrene for Sheet Extrusion Product Description: High Impact Polystyrene PS 330 is manufactured by continuous mass polymerization of styrene monomer. An elastomer is incorporated during polymerization to achieve impact resis.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895B |
Total Finaprene® 602D Clear Impact Polystyrene
(discontinued **) Finaprene® 602D is a clear high styrenic styrene-butadiene (SBS) block copolymer with a radial structure, which is widely used as modifiers or in alloys with many plastic resins, such polystyrene, .. |
|||
Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Magyar Aluminum ALO-P54-04 Alumina Alumina for Polishing |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | DIN-53466 |
Iran Petrochemical (PCC) PVC-S6558 Poly Vinyl Chloride Grade S6558 has low porosity & high bulk density.Applications: pipe and fitting, injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 60 |
Lanxess Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.600 - 1.00 g/cc | 0.0217 - 0.0361 lb/in³ | tapped |
Solvay Chemicals Barium carbonate fine powder Barium carbonate fine powder is specially developed for usage in the brick and tile industry and for the removing of sulfates. Other applications are in the ceramic and ferrite industry. It is also .. |
|||
Bulk Density | 0.601 g/cc | 0.0217 lb/in³ | Dry |
Skamol Group SKAMOLEX V-1100 (600) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Solvay REPEL-O-TEX® SRP-6 Polyethylene Glycol Polyester Description: Soil Release Polymer offering protection against the adhesion of greasy soils between two wash cycles. 100% active material in powder form.Chemical Name: POLYETHYLENE GLYCOL POLYESTERCA.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plenco 2369 Phenolic, Granular, Injection Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plenco 2408 Phenolic, Granular, Compression Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plenco 7100 Phenolic, Nodular, Injection Molded PLENCO 07100 is an organic fiber reinforced phenolic molding compound, with improved mechanical strength properties and an industrial finish. 07100 is densified for easy handling and good pourabilit.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plenco 7507 Phenolic, Granular, Compression Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | Size D (apparent) |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | Powder Density; ISO 60 |
Vyncolit X6151 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Highest impact, high strain to failure, glycol resistant.USES: Water pumps and water pump .. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 1183 |
Polyram RamClean™ 101 Purging Agent Purging agent for injection molding machines.Information provided by Polyram. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plenco 2408 Phenolic, Granular, Injection Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Bulk Density | 0.600 - 0.750 g/cc | 0.0217 - 0.0271 lb/in³ | Powder Density; ISO 60 |
Vyncolit 2950 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 60 |
Vyncolit Neopreg Kinel® SK4503 S5 Aramid Reinforced Molding Compound Long aramid fiber reinforced BMI molding compound suited for very demanding tribologic applications under medium to poor lubricated conditions, high temperatures & PV levelsInformation provided by S.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Neopor® 5300 Plus Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Peripor® 200 Expandable Polystyrene Description: Expandable polystyrene (EPS) with uniformly distributed flame retardant (blowing agent: pentane)Remarks: Low-pentane products for the production of flame-retardant foams displaying low .. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Styropor® F 395 -N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Axion Polymers Axplas® PS07 0000 General Purpose Polystyrene PS07 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS07 range of resin co.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Styropor® F 495-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Styropor® P 226 C Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Blocks with very short cycle times.Info.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Styropor® P 656 Expandable Polystyrene Additive Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: Filling material for lightweight plasters.Information provided .. |