Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.548 - 0.646 g/cc | 0.0198 - 0.0233 lb/in³ | |
Suqian Unitechem Light Stabilizer 944 Chemical Name: Poly-{[6-[(1,1,3,3-tetramethylbutyl)amino]-1,3,5-triazine-2,4-diyl][(2,2,6,6-tetramethyl-4-piperidyl)imino]-1,6-hexanediyl[(2,2,6,6-tetramethyl-4-piperidyl)imino]}CAS NO.: 70624-18-9M.. |