Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.545 g/cc | 0.0197 lb/in³ | Dry |
Skamol Group ISOPERLOR 550P Perlite Insulating Brick & Block ISOPERLOR perlite insulating bricks & blocks have the following characteristics: Max. service temperature 900°C (1652°F)Back-up insulation onlyExcellent insulating propertiesVery lightweight a.. |
|||
Bulk Density | 0.545 g/cc | 0.0197 lb/in³ | As Supplied |
Skamol Group Moler BB-Filler Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Bulk Density | 0.545 g/cc | 0.0197 lb/in³ | Dry |
Skamol Group Moler HIPOR Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Bulk Density | 0.545 g/cc | 0.0197 lb/in³ | As Supplied |
Skamol Group SKAMOCAST 112-80 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Bulk Density | 0.545 g/cc | 0.0197 lb/in³ | Loose |
CIMBAR RiverCal™ 8103 & 8103C Calcium Carbonate (CaCO3) RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications.. |