Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total Lumicene® MR30MC2 Metallocene Random Copolymer Polypropylene, Injection Molding Lumicene® MR30MC2 is a metallocene random copolymer with a melt flow index of 30 g/10 min for injection molding. Lumicene® MR30MC2 differs from the other random copolymers by its molding reproduci.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10642 is characterized by high fluidity with good mechanical prope.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 11712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 11712 is a nucleated controlled-rheology heterophasic copolymer. PPC 11712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 3660 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 3660 is an heterophasic copolymer. PPC 3660 is characterized by a low fluidity hence good melt strength to provide east of processing and good manufactured article propert.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 3666 Polypropylene, Heterophasic Copolymer, Extrusion Polypropylene PPC 3666 is a heterophasic copolymer with a Melt Flow index of 1.5 g/10 min. This resin offers an outstanding processability in combination with good melt strength and excellent mecha.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 5752 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 5752 is a nucleated controlled-rheology heterophasic copolymer. PPC 5752 is characterized by a high impact resistance and excellent antistatic properties. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 7612 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7612 is a nucleated and controlled-rheology heterophasic copolymer. PPC 7612 is characterized by a good balance between rigidity and impact resistance and has excellent antistatic.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 7642 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7642 is a nucleated and antistatic heterophasic copolymer. PPC 7642 is characterized by a very high stiffness. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 7652 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 7652 is a nucleated and antistatic heterophasic copolymer with a Melt Flow index of 16 g/10 min.Polypropylene PPC 7652 is a medium flow grade intended for a wide range of injection.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 7760 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7760 is a heterophasic copolymer. PPC 7760 is characterized by medium fluidity offering a combination of ease of processing and excellent impact properties in applications ranging.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 9612 Polypropylene, Heterophasic Copolymer, Injection Molding This product is a Total Ecosolutions grade.Polypropylene PPC 9612 has been developed specifically for the injection molding of crates and is characterized by a high Melt Flow index of 20 g/10 min. .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 9760 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9760 is heterophasic copolymer. PPC 9760 is characterized by improved stiffness, creep resistance and high impact resistance. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 12020 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 12020 is a clarified high fluidity homopolymer with a melt flow index of 60 g/10 min.Polypropylene PPH 12020 has been designed with a very high stiffness and an outstanding transpa.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 3150 Polypropylene, Homopolymer Polypropylene PPH 3150 is a modified homopolymer polypropylene with a Melt Flow index of 2 g/10 min.Polypropylene PPH 3150 is intended for the production at very high speed of flat bioriented films .. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | Internal |
Total PPH 3862 Homopolymer Polypropylene, Fiber Grade Total Petrochemicals Polypropylene 3862 is recommended for high speed melt spinning processes and multifilament yarns like bulk continuous filament (BCF) and continuous filament (CF) fibers. 3862 i.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4022 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4022 is a clarified nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4022 has been developed for extrusion-thermoforming, providing improved rigidity and impact r.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4054 Polypropylene Homopolymer Polypropylene PPH 4054 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4054 has been designed for the production of BOPP film with the tenter frame process. Th.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4060 is homopolymer.ApplicationATOFINA Polypropylene PPH 4060 is specially suitable for tape extrusion for woven applications and for extrusion thermoforming. PPH 4060 is.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 4069 Polypropylene Homopolymer, Fiber Polypropylene PPH 4069 is a homopolymer polypropylene with a Melt Flow index of 4 g/10 min.Polypropylene PPH 4069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 6080 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6080 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 7069 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7069 is homopolymer.ApplicationATOFINA Polypropylene PPH 7069 is characterized by medium fluidity for extrusion of continuous filament (CF) and bulk continuous filament (BC.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 9040 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9040 is a nucleated homopolymer. PPH 9040 is characterized by an improved rigidity and high clarity .ApplicationATOFINA Polypropylene PPH 9040 is suitable for the injectio.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPH 9081 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9081 is a controlled-rheology homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing improved impact res.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPM R020 Polypropylene, Random Copolymer for Medical Grade Polypropylene PPM R020 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 11750 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11750 is a nucleated and controlled-rheology heterophasic copolymer with very high Melt Flow index of 50 g/10 min.Polypropylene PPC 11750 is characterized by good impact resistance.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 2660 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 2660 is a heterophasic copolymer. PPC 2660 is characterized by a low fluidity hence good melt strength to provide ease of processing and good manufactured article properti.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPC 3650 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 3650 is a heterophasic copolymer with a Melt Flow index of 2 g/10 min.Polypropylene PPC 3650 provides an excellent balance between toughness and flow, being particularly suitable i.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPR 3261 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3261 is a high melt strength random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals... |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPR 6288 Random Copolymer Polypropylene, Cast Extrusion of Film Total Petrochemicals PPR 6288 is a random copolymer polypropylene with a melt flow index of 8 g/10 min for the cast extrusion of films with outstanding optical properties and easy heat weldability.P.. |
|||
Bulk Density | 0.525 g/cc | 0.0190 lb/in³ | ISO 1183 |
Total PPR 3260 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3260 is a random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals. |