Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Loose |
Nyco NYAD® G Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
Nabaltec ACTILOX® B60 AS1 AlO(OH) Boehmite Surface treated flame retardant filler with reduced particle size and optimized viscosity in engineering plastics for synergistic effects with other flame retardants.Properties:Very fine product in .. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
PolyOne Geon™ 180 Series 186A Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 186A is low molecular weight homopolymer resin, providing a good balance of fused film physical properties and fusion characteristics. It provides excellent chemical foam characteristics with.. |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
Magyar Aluminum ALO-P90-06 Alumina Alumina for Polishing |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
Magyar Aluminum ALO-P95-08 Alumina Alumina for Polishing |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D 1895 method B |
Kraton® D1101 E (SBS) Liner Block Copolymer Description: Kraton D1101 E polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D 1895 method B |
Kraton® D1186 A (SBS) Branched Block Copolymer Description: Kraton D1186 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D 1895 method B |
Kraton® D1189 A (SBS) Radial Block Copolymer Description: Kraton D1189 A is a clear, radial block copolymer based on styrene and butadiene with bound styrene of 32% mass. It is supplied from Europe in the physical forms indicated in the grade .. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D 1895 method B |
Kraton® D1191 E (SBS) Radial Block Copolymer Description: Kraton D1191 E is a clear, radial block copolymer based on styrene and butadiene with bound styrene of 33.5% mass. It is supplied from Europe in the physical forms described: Kraton D11.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D 1895 method B |
Kraton® D1192 A (SBS) Liner Block Copolymer Description: Kraton D1192 A is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms described: Kraton D1192 .. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D 1895 method B |
Kraton® D1192 B (SBS) Liner Block Copolymer Description: Kraton D1192 B is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from South America in the physical form described: Kraton .. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | ASTM D 1895 method B |
Kraton® D4153 E (O/E SBS) Linear Block Copolymer Description: Kraton D4153 E is an oil-extended linear block copolymer based on styrene and butadiene with bound styrene in the neat polymer of 35% mass. It contains 40 phr paraffinic oil which is cl.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Tap Density |
Momentive Performance Materials AC6041 Boron Nitride (BN) Powder Crystalline hexagonal platelet morphology. AC6041 shows good dispersion, with enhanced lubricity and thermal properties. AC6041 powder is readily used in the production of many advanced materials... |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Tap Density |
Momentive Performance Materials PolarTherm® PT131 Boron Nitride (BN) Powder Boron Nitride powders are produced by GE Advanced Ceramics in more than 50 individual (standard and custom) grades to meet a wide variety of application needs.For use in: Electrically insulating/the.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ 350 Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ FM-1 Hollow Spheres EXTENDOSPHERESâ„¢FM-1 ceramic hollow spheres are a low-density functional additive for disc brake pads, truck and train blocks, clutch facings and other friction materials. They are compatible wi.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ SG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Apparent |
Shin-Etsu Silicones KSP-100 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
Solvay GEROPON® TA/72 Surfactant Identification: SODIUM POLYCARBOXYLATESolubility: Soluble in water. Insoluble in polar and aromatics solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Dispers.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America RX® 431 Cellulose Reinforced Phenolic Novolac RX431 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac RX448 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
Solvay SUPRAGIL® MNS/90 Condensed methyl naphthalene sulfonate, sodium salt Condensed methyl naphthalene sulfonate, sodium salt. High performance, non-foaming, dispersing agent for wide range of applications, binding properties. Specific to high conc. WG.Identification: POL.. |
|||
Bulk Density | 0.400 - 0.480 g/cc | 0.0145 - 0.0173 lb/in³ | |
Trelleborg Fillite® 160W Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.400 - 0.480 g/cc | 0.0145 - 0.0173 lb/in³ | |
Trelleborg Fillite® SGHA (500HA) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.400 - 0.561 g/cc | 0.0145 - 0.0203 lb/in³ | Dow Method |
Dow Saran® 506 Polymer Saran™ 506 Polymer is designed as an ignition resistant adhesive bonding agent. Saran™ 506 is a vinylidene chloride copolymer supplied as a white, micronized powder. It is unaffected by humidity.. |
|||
Bulk Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | |
BASF Hydroxypivalic Acid Neopentylglycolester (HPN Formula: C10H20O4CAS: 1115-20-4Description: Hydroxypivalic Acid Neopentylglycolester (HPN) is a colorless, odorless solid.Synonyms: Neopentyl glycol monohydroxypivalate, Hydroxyneopentyl hydroxypiva.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
BASF Heligoen® Blue K 6850 Color Additive Chemical Structure: Cu-Phthalocyanine alpha instab.Application: Colourant for plastics; PVC-p, PVC-u and UPRecommendations for food applications: BgVV, FDA, FrancePhysical form: PowderInformation pr.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
BASF Heligoen® Green K 9360 Color Additive Chemical Structure: Cu-phthalocyanine halogenisedApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PETP, CA/CAB, and UPRecommendations for food application.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
Nabaltec ACTILOX® B60 AlO(OH) Boehmite Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature stabilitySynergistic effects with other flame retardantsHigh acid resistance.. |
|||
Bulk Density | 0.400 g/cc | 0.0145 lb/in³ | |
Nabaltec APYRAL® 40CD Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |