Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.310 g/cc | 0.0112 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons ECORAX® 1670 Carbon Black Specialty black for tire treads and bodies that provide reduced rolling resistanceInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.310 - 0.410 g/cc | 0.0112 - 0.0148 lb/in³ | ASTM D1895 |
LG Chemical PB1120 PVC General Description: PB1120, homopolymer made by micro-suspension seeded polymerization, is medium-viscosity PVC resin with pseudo plastic flow property. It can be used for foam flooring layer and w.. |
|||
Bulk Density | 0.310 - 0.410 g/cc | 0.0112 - 0.0148 lb/in³ | ASTM D1895 |
LG Chemical PB1202 PVC General Description: PB1202, homopolymer made by micro-suspension seeded polymerization, PVC Resin has a fluid property similar to Newtonian fluidity (low-viscosity) It is mainly used for non-foamin.. |
|||
Bulk Density | 0.310 - 0.410 g/cc | 0.0112 - 0.0148 lb/in³ | ASTM D1895 |
LG Chemical PB1302 PVC General Description: PB1302, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for ca.. |
|||
Bulk Density | 0.310 - 0.410 g/cc | 0.0112 - 0.0148 lb/in³ | ASTM D1895 |
LG Chemical PE1311 PVC General Description: PE1311, homopolymer made by emulsion polymerization, is a high-viscosity PVC resin with pseudo-plastic flow property PE1311 has an good chemical foaming with low density and fin.. |
|||
Bulk Density | 0.310 - 0.350 g/cc | 0.0112 - 0.0126 lb/in³ | |
Solvay AG-RHOâ„¢ DEP-775 Surfactant Description: Anti-drift agent as adjuvants or to formulate into plant protection productsIdentification: DERIVATIZED NATURAL POLYMER CAS: 497-19-8 Water Solubility: Quick hydrationAvailable in: Asia.. |
|||
Bulk Density | 0.310 g/cc | 0.0112 lb/in³ | |
Zircar Ceramics ECO-1200A Alumina-Silica Insulation This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-1200 is part of hundreds of different thermal process systems. Information provid.. |
|||
Bulk Density | 0.310 g/cc | 0.0112 lb/in³ | |
DuPont™ Nomex® 411 Paper, 10 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Bulk Density | 0.310 g/cc | 0.0112 lb/in³ | |
DuPont™ Nomex® 411 Paper, 15 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Bulk Density | 0.310 g/cc | 0.0112 lb/in³ | |
DuPont™ Nomex® 411 Paper, 23 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Bulk Density | 0.310 g/cc | 0.0112 lb/in³ | |
DuPont™ Nomex® 411 Paper, 7 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |