Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.250 g/cc | 0.00903 lb/in³ | ISO 1183 |
Victrex® PEEK 600PF Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact complian.. |
|||
Bulk Density | 0.250 - 0.400 g/cc | 0.00903 - 0.0145 lb/in³ | |
Magyar Aluminum ALOLT 120F Aluminum Hydroxide Fine Precipitated Type |
|||
Bulk Density | 0.250 - 0.500 g/cc | 0.00903 - 0.0181 lb/in³ | |
Magyar Aluminum ALOLT 60F Aluminum Hydroxide Fine Precipitated Type |
|||
Bulk Density | 0.250 - 0.450 g/cc | 0.00903 - 0.0163 lb/in³ | |
Magyar Aluminum ALOLT 90DLS Aluminum Hydroxide Fine Precipitated Type |
|||
Bulk Density | >= 0.250 g/cc | >= 0.00903 lb/in³ | Aerated; LSY-QB-KD019 |
LG Chemical EM500 Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Bulk Density | >= 0.250 g/cc | >= 0.00903 lb/in³ | Aerated; LSY-QB-KD019 |
LG Chemical EM500A Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Bulk Density | >= 0.250 g/cc | >= 0.00903 lb/in³ | Aerated; LSY-QB-KD019 |
LG Chemical EM505 Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Bulk Density | 0.250 g/cc | 0.00903 lb/in³ | Tap Density |
Momentive Performance Materials NX5 Boron Nitride (BN) Powder Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.NX grades a.. |
|||
Bulk Density | 0.250 - 0.300 g/cc | 0.00903 - 0.0108 lb/in³ | |
Sinotek Materials Rigid Graphite Felt Board Heat Insulation Material Information provided by Sinotek |
|||
Bulk Density | 0.250 g/cc | 0.00903 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America E 264H Long Glass Fiber Reinforced Epoxy E 264H is a high strength, long fiberglass reinforced epoxy molding compound, which features improved flow in transfer molding.Information provided by Sumitomo Bak North America, Inc. |
|||
Bulk Density | 0.250 g/cc | 0.00903 lb/in³ | |
Zircar Zirconia ZYBF-5 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |
|||
Bulk Density | 0.250 g/cc | 0.00903 lb/in³ | |
Chosun Refractories 1000BOARD Board Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.250 g/cc | 0.00903 lb/in³ | |
Chosun Refractories 1260BOARD Board Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.250 - 0.300 g/cc | 0.00903 - 0.0108 lb/in³ | |
BASF Ultrason® E 2020 P SR PESU Description: Polyethersulfone flakes, e.g. for membrane applications, coatings and resin modification, containing min. 50% of OH-endgroups. The product is soluble in N-methyl-pyrrolidone (NMP) and N.. |
|||
Bulk Density | 0.250 g/cc | 0.00903 lb/in³ | ASTM D4895 |
3M Dyneon™ J14 PTFE Micropowder 3M™ Dyneon™ PTFE Micropowders can be used as additives in many applications and at concentrations typically from 5 to 20%. Homogeneous incorporation is the single most important process and applic.. |
|||
Bulk Density | 0.250 g/cc | 0.00903 lb/in³ | |
Zircar Zirconia ZYBF-5 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |