Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.170 g/cc | 0.00614 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-150 Hollow Spheres EXTENDOSPHERESâ„¢ XOL-150 are white aluminosilicate multicellular hollow spheres. The density of this product is 0.30 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-150 hollo.. |
|||
Bulk Density | 0.170 g/cc | 0.00614 lb/in³ | Scott, Typical |
TIMCAL TIMREX® LSG 44 Natural Graphite Flakes TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |