Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.160 - 0.192 g/cc | 0.00579 - 0.00694 lb/in³ | Loose |
KaMin Polygloss® 90 Kaolin Clay - Ultrafine, high brightness Ultrafine, highly pulverized, premium brightness kaolin for extending high gloss solvent and water-based coatings.Industry: Paint & Coatings, Rubber & Plastic, InkUses: Architectural Coatings, Indus.. |
|||
Bulk Density | 0.160 g/cc | 0.00579 lb/in³ | Loose |
CIMBAR FlexTalc® 815 Ultrafine Talc for TPO Applications Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprieta.. |