Physical Properties Metric English Comments
Bulk Density 0.0333 g/cc
0.00120 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN LSP-30EB Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0333 g/cc
0.00120 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN OP-30DB Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0333 g/cc
0.00120 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN OP-30E Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0333 g/cc
0.00120 lb/in³
After expansion
Sekisui PIOCELAN OP-30EU (Low VOC, Low odor) Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0333 g/cc
0.00120 lb/in³
After expansion
Sekisui PIOCELAN OP-E30ENS (Antistatic) Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0333 g/cc
0.00120 lb/in³
After expansion; ASTM D3575