Polymer Property : Bulk Density = 0.000903 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.0250 g/cc
0.000903 lb/in³
Minimum
SYNTHOS Koplen® 0207 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into thin walled products.Specific Characteristics: Flammability according ..
Bulk Density 0.0250 - 0.0600 g/cc
0.000903 - 0.00217 lb/in³
Typical
SYNTHOS Koplen® 0207 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into thin walled products.Specific Characteristics: Flammability according ..
Bulk Density >= 0.0250 g/cc
>= 0.000903 lb/in³
Typical
SYNTHOS Koplen® 0207 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to thin-wall moldings. Lower density can be achie..
Bulk Density 0.0250 g/cc
0.000903 lb/in³
Minimum
SYNTHOS Koplen® 0814 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to molded bricks and blocks. Lower density can be..
Bulk Density 0.0250 g/cc
0.000903 lb/in³
Minimum
SYNTHOS Koplen® 0822 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to molded bricks and blocks. Lower density can be..
Bulk Density 0.0250 g/cc
0.000903 lb/in³
Minimum
SYNTHOS Koplen® 2040 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks. Lower density can be achieved after several prefor..
Bulk Density 0.0250 g/cc
0.000903 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN LP-40E Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0250 g/cc
0.000903 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN LSP-40EB Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0250 g/cc
0.000903 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN SP-40D Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0250 g/cc
0.000903 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN SP-40E Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0250 g/cc
0.000903 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN TOPF-40DB Flame Retardant Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0250 g/cc
0.000903 lb/in³
After expansion
Sekisui PIOCELAN TOPF-40DUB Black (Low VOC, Low odor) Flame Retardant Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..