Physical Properties Metric English Comments
Bulk Density 0.0200 - 0.0400 g/cc
0.000723 - 0.00145 lb/in³
Typical
SYNTHOS Koplen® 2040 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks.Specific Characteristics: Flammability according to CSN EN ISO ..
Bulk Density 0.0200 g/cc
0.000723 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN LP-50E Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0200 g/cc
0.000723 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN LSP-50EB Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0200 g/cc
0.000723 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN SP-50D Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0200 g/cc
0.000723 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN SP-50E Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..