Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0190 - 0.390 g/cc | 0.000686 - 0.0141 lb/in³ | Dependent on grade. |
Destech Open-Celled Glassy Carbon Foam Destech glassy (vitreous) carbon foam is available in different grades depending on the number of pores per inch (ppi). Standard grades are 10, 45, 100 and 500 ppi. Custom grades are available on a.. |
|||
Bulk Density | 0.0190 - 0.0232 g/cc | 0.000686 - 0.000838 lb/in³ | |
BASF Neopolen® P 8225 K 0.025 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Bulk Density | 0.0190 - 0.0232 g/cc | 0.000686 - 0.000838 lb/in³ | |
BASF Neopolen® P 8225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Bulk Density | 0.0190 - 0.0232 g/cc | 0.000686 - 0.000838 lb/in³ | |
BASF Neopolen® P 8225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Bulk Density | 0.0190 - 0.0232 g/cc | 0.000686 - 0.000838 lb/in³ | |
BASF Neopolen® P 8225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |