Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0180 g/cc | 0.000650 lb/in³ | Minimum |
SYNTHOS Koplen® 0513 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into moldings and smaller blocks.Specific Characteristics: Flammability acc.. |
|||
Bulk Density | 0.0180 - 0.0400 g/cc | 0.000650 - 0.00145 lb/in³ | Typical |
SYNTHOS Koplen® 0513 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into moldings and smaller blocks.Specific Characteristics: Flammability acc.. |
|||
Bulk Density | >= 0.0180 g/cc | >= 0.000650 lb/in³ | Typical |
SYNTHOS Koplen® 0513 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: Expansion of beads by water steam, hot water or hot air. Shaping into products and smaller blocks. Lower density can be achieved aft.. |
|||
Bulk Density | 0.0180 g/cc | 0.000650 lb/in³ | Minimum |
SYNTHOS Koplen® 2040 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks.Specific Characteristics: Flammability according to CSN EN ISO .. |
|||
Bulk Density | 0.0180 - 0.0350 g/cc | 0.000650 - 0.00126 lb/in³ | |
BASF Styropor® KF 462M EPS Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 18-35 kg/m3 and fire characteristics in conformity with.. |