Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 90 PF Moldable Refractory Material Description: Curas 90 PF ramming mix with outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). The product is supplied in two components: a dry powder and a liquid. Curas 90 PF i.. |
|||
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 180 Dense Refractory Castable Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th.. |
|||
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | After drying at 110°C |
Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values .. |
|||
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable Description: Vibron 130 is a vibrating castable with a low cement content, based on abrasion resistant spinel grains.Remarks: Indicated values apply to vibrated products.Information provided by Goud.. |
|||
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid.. |
|||
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | |
Chosun Refractories BATN-3 Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.75 - 2.85 g/cc | 0.0994 - 0.103 lb/in³ | |
Chosun Refractories BATN-D2, Upper Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |