Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.40 - 1.50 g/cc | 0.0506 - 0.0542 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 130 GM Refractory Insulating Castable Description: Golite 130 GM is a standard, medium weight gunning castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast p.. |
|||
Bulk Density | 1.40 - 1.50 g/cc | 0.0506 - 0.0542 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 130 Refractory Insulating Castable Description: Golite 130 is a standard, medium weight castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast products. Al.. |
|||
Bulk Density | 1.40 - 1.50 g/cc | 0.0506 - 0.0542 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Rema.. |