Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9212 E Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9216 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.20 - 1.35 g/cc
0.0434 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9510 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9612 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9620 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9622 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.20 - 1.35 g/cc
0.0434 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9634 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9816 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9923 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Copyright © lookpolymers.com All Rights Reserved