Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Nabaltec GRANALOX® NM 9916 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.00 - 1.20 g/cc | 0.0361 - 0.0434 lb/in³ | |
Nabaltec NABALOX® NO 615-30 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 1.00 - 1.20 g/cc | 0.0361 - 0.0434 lb/in³ | |
Nabaltec NABALOX® NO 625-30 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 1.00 - 1.20 g/cc | 0.0361 - 0.0434 lb/in³ | |
Nabaltec NH 20 Aluminum Hydroxide Used in the production of glass and ceramic productsaluminum fluoride, cryolite and other aluminum saltsfrits and pigmentsmolecular sievescatalystsrefractory productspigments |
|||
Bulk Density | 0.500 - 1.20 g/cc | 0.0181 - 0.0434 lb/in³ | Apparent Density |
Indium Corp. Standard ITO Indium Tin Oxide Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo.. |
|||
Bulk Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Inhance Fluoro-Seal INHANCE® Ti-9000 Titanium Carbide Product Description: INHANCE Ti-9000 consists of spherically shaped titanium carbide micro grains. This product is used to make other INHANCE polymer alloys. When incorporated in polymers, unique .. |
|||
Bulk Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Inhance Fluoro-Seal INHANCE® Ti-9100 Titanium Carbide Polymer Alloy Product Description: INHANCE Ti-9100 polymer alloy consists of spherically shaped titanium carbide micro grains coated with a thin layer of a proprietary coupling agent. This product was designed .. |
|||
Bulk Density | 0.500 - 1.20 g/cc | 0.0181 - 0.0434 lb/in³ | Apparent Density |
Indium Corp. Fine ITO Indium Tin Oxide Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo.. |
|||
Bulk Density | 0.600 - 1.20 g/cc | 0.0217 - 0.0434 lb/in³ | |
Solvay Chemicals NOCOLOK® Zn Flux Reactive flux alternative to arc spray Zn coating.HS No.: 38109090 /CAS-No.: 13827-02-6Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical .. |
|||
Bulk Density | 0.900 - 1.20 g/cc | 0.0325 - 0.0434 lb/in³ | |
Solvay Chemicals Oxyper® S131 Sodium Percarbonate Oxyper® S131 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products and environmental applications; it may be suitabl.. |
|||
Bulk Density | 0.900 - 1.20 g/cc | 0.0325 - 0.0434 lb/in³ | |
Solvay Chemicals Oxyper® S142 Sodium Percarbonate Oxyper® S142 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in formulated bleach additive products, detergent powders and tablets, automa.. |
|||
Bulk Density | 0.900 - 1.20 g/cc | 0.0325 - 0.0434 lb/in³ | |
Solvay Chemicals Oxyper® SHC Sodium Percarbonate Oxyper® SHC is a high coated, stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products, detergent powders and tablets, autom.. |
|||
Bulk Density | 1.00 - 1.20 g/cc | 0.0361 - 0.0434 lb/in³ | 540MA3C63 |
Solvay MIRAPOL® SURF-S 411 HA Surfactant Description: Rinse aid polymer specially formulated for auto dish wash powders and tablets. Recommended as a substitute to rinse aid surfactants. Enables raw material cost saving, while boosting rin.. |
|||
Bulk Density | 0.800 - 1.20 g/cc | 0.0289 - 0.0434 lb/in³ | |
Solvay Chemicals (CsAlF-Complex) Cesium Fluoroaluminate Low-melting-point flux for brazing aluminum.HS No.: 38109090 /CAS-No.: 138577-01-2 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical Appl.. |