Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.800 - 1.05 g/cc | 0.0289 - 0.0379 lb/in³ | |
Magyar Aluminum ALO-DF223 Alumina Alumina for Polishing |
|||
Bulk Density | 0.900 - 1.05 g/cc | 0.0325 - 0.0379 lb/in³ | Powder Density; ISO 60 |
Vyncolit X658 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by .. |