Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 105 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 105 RA Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 201 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 713-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 713-40 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 715-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 725-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.700 - 1.00 g/cc | 0.0253 - 0.0361 lb/in³ | |
Magyar Aluminum ALO-DFM Alumina Alumina for Polishing |
|||
Bulk Density | 0.600 - 1.00 g/cc | 0.0217 - 0.0361 lb/in³ | tapped |
Solvay Chemicals Barium carbonate fine powder Barium carbonate fine powder is specially developed for usage in the brick and tile industry and for the removing of sulfates. Other applications are in the ceramic and ferrite industry. It is also .. |