Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.850 - 0.950 g/cc | 0.0307 - 0.0343 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-109JS PET Sheet Grade Used mainly for 5 to 20 liter mineral water containers |
|||
Bulk Density | 0.850 - 0.950 g/cc | 0.0307 - 0.0343 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-113C PET Sheet Grade Used mainly for box strapping. |
|||
Bulk Density | 0.700 - 0.950 g/cc | 0.0253 - 0.0343 lb/in³ | |
Magyar Aluminum ALO-P54 Alumina Alumina for Polishing |
|||
Bulk Density | 0.850 - 0.950 g/cc | 0.0307 - 0.0343 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati.. |
|||
Bulk Density | 0.850 - 0.950 g/cc | 0.0307 - 0.0343 lb/in³ | DIN 53466 |
Stanelco Bioplast® Wrap 100 Biodegradable Plastic Bioplast Wrap 100 is a plasticiser-free thermoplastic material which allows the production of films with coated paper-like properties. Wrap 100 is an excellent, eco-friendly alternative to laminated.. |
|||
Bulk Density | 0.750 - 0.950 g/cc | 0.0271 - 0.0343 lb/in³ | Powder Density; ISO 60 |
Vyncolit 3640 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |