Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.320 - 0.480 g/cc | 0.0116 - 0.0173 lb/in³ | |
Protective Coating PC-Wood Guardian™ Wood Preservative PC-Wood Guardian™ isused in preventing and controlling decay fungi. It is an effective treatment for wood and wood composite to kill and prevent infestations of decay fungi including white and brow.. |
|||
Bulk Density | 0.400 - 0.480 g/cc | 0.0145 - 0.0173 lb/in³ | |
Trelleborg Fillite® 160W Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.400 - 0.480 g/cc | 0.0145 - 0.0173 lb/in³ | |
Trelleborg Fillite® SGHA (500HA) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.400 - 0.480 g/cc | 0.0145 - 0.0173 lb/in³ | |
Trelleborg Fillite® 300W Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.400 - 0.480 g/cc | 0.0145 - 0.0173 lb/in³ | Dried |
Zircar Ceramics SALI Moldable Alumina Insulation A close cousin to premium grade Type SALI insulation, SALI Moldable is a thick doughy material readily shaped into complex forms using molds & hand building techniques or applied to surfaces. When .. |
|||
Bulk Density | 0.380 - 0.480 g/cc | 0.0137 - 0.0173 lb/in³ | Tap; ASTM D4164 |
CRP Technology Windform® PS Polystyrene for Selective Laser Sintering Windform® PS is a polystyrene based material, developed specifically to produce complex investment casting patterns. The sintered patterns are ideal for conventional wax infiltration, and become ea.. |
|||
Bulk Density | 0.400 - 0.480 g/cc | 0.0145 - 0.0173 lb/in³ | |
Akzo Nobel Expancel® 092 MB 120 Masterbatch with unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |