Physical Properties Metric English Comments
Bulk Density 2.45 - 2.55 g/cc
0.0885 - 0.0921 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 160 Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and maintains its strength up to high temperatures. In addition Curon 160 has an excellent thermal sh..
Bulk Density 2.45 - 2.55 g/cc
0.0885 - 0.0921 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 180 L Dense Refractory Castable
Description: Curon 180 L is a castable based on fused alumina for use up to 1800°C and shows a good thermal shock resistance.Remarks: These values apply to cast products. Also available in gunnin..
Bulk Density 2.45 - 2.55 g/cc
0.0885 - 0.0921 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable
Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib..
Bulk Density 2.45 - 2.55 g/cc
0.0885 - 0.0921 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 160 H SiC Dense Vibrating Refractory Castable
Description: Vibron 160 H SiC is a low cement vibrating castable characterized by a high strength, good abrasion resistance and excellent thermal shock resistance. Because of the presence of SiC, th..
Bulk Density 2.45 g/cc
0.0885 lb/in³
Chosun Refractories CRAG-S27 Long Stopper
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.45 g/cc
0.0885 lb/in³
Chosun Refractories SBSN20 Nozzle
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.45 g/cc
0.0885 lb/in³
Chosun Refractories TD-165H Special Casting Block
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved