Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.33 g/cc | 0.0842 lb/in³ | |
Du-Co Ceramics S-464 Magnesia Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
Bulk Density | 2.33 g/cc | 0.0842 lb/in³ | |
Chosun Refractories SF35 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.33 g/cc | 0.0842 lb/in³ | |
Chosun Refractories H-4S High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |