Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.86 g/cc | 0.0671 lb/in³ | Dipping, 10% H2O |
BNZ Materials Zelie No. 20 Mortar No. 20 is an air-setting mortar, gray in color, for use where extra hard air-set strength is desired. It is not recommended for laying insulating fire brick. Used up to 2700°F for setting hard bric.. |
|||
Bulk Density | 1.86 g/cc | 0.0671 lb/in³ | Powder |
Aremco Ceramacast™ 646-N High Temperature Potting & Casting Material Zirconia Castable ceramic with high dielectric and physical strength. |