Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.40 g/cc | 0.0506 lb/in³ | Loose |
Nyco HARRP™ 20 X 40 Wollastonite HARRP™ 20X40 is suggested for concrete and concrete roof tile reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive.. |
|||
Bulk Density | 1.40 - 1.60 g/cc | 0.0506 - 0.0578 lb/in³ | JIS K5101 |
NYC YT3WBHQ Y2O3 Powder for Spray Coating High purity granules produced in clean environment. Uses include semiconductor / LCD industries and electroceramics.Narrow particle size distributionTailorable for each spray coating technologyNo c.. |
|||
Bulk Density | 1.40 g/cc | 0.0506 lb/in³ | Tap Density of Granules |
NYC YT3WBQ Y2O3 CIP (Cold Isostatic Pressing) Granules 99.9% and better high purity granules produce high quality finished ceramics. Uses include semiconductors / LCD industries, metallurgy, magnets, and electroceramics.Acrylic binder systemExcellent g.. |
|||
Bulk Density | 1.40 g/cc | 0.0506 lb/in³ | |
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and mos.. |
|||
Bulk Density | <= 1.40 g/cc | <= 0.0506 lb/in³ | |
Magyar Aluminum ALOLT 01 Aluminum Hydroxide Dry type |
|||
Bulk Density | 1.40 g/cc | 0.0506 lb/in³ | |
MarkeTech Repton 931 Cordierite Mg-Al-Si Oxide REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Bulk Density | 1.40 g/cc | 0.0506 lb/in³ | Tap Density; ASTM B527 |
H.C. Starck FeCoCu Prealloyed Metal Powder A new prealloyed metallic powder of high sinter-activity with ideally homogenized constituents at an atomic level. The primary particles of very fine grain size are loosely agglomerated to agglomera.. |
|||
Bulk Density | 1.40 - 1.50 g/cc | 0.0506 - 0.0542 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 130 GM Refractory Insulating Castable Description: Golite 130 GM is a standard, medium weight gunning castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast p.. |
|||
Bulk Density | 1.40 - 1.50 g/cc | 0.0506 - 0.0542 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 130 Refractory Insulating Castable Description: Golite 130 is a standard, medium weight castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast products. Al.. |
|||
Bulk Density | 1.40 g/cc @Temperature 200 °C |
0.0506 lb/in³ @Temperature 392 °F |
|
Sharadaa Ceramics Sharada LTM 1.4 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | 1.40 g/cc | 0.0506 lb/in³ | Size B (tapped) |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 1.40 g/cc | 0.0506 lb/in³ | Size B (tapped) |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 1.40 g/cc | 0.0506 lb/in³ | |
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and mos.. |
|||
Bulk Density | 1.40 - 1.50 g/cc | 0.0506 - 0.0542 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Rema.. |