Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | |
Nabaltec GRANALOX® NM 9620 F Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | |
Nabaltec GRANALOX® NM 9922 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | <= 1.15 g/cc | <= 0.0415 lb/in³ | |
Magyar Aluminum ALOLT 21AF Aluminum Hydroxide Ground type |
|||
Bulk Density | 1.15 - 1.25 g/cc | 0.0415 - 0.0452 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 135 RL C Refractory Insulating Castable Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast .. |
|||
Bulk Density | 1.15 g/cc | 0.0415 lb/in³ | |
DuPont™ Nomex® 418 Paper, 8 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Bulk Density | 1.15 g/cc | 0.0417 lb/in³ | |
CIMBAR Suspengel™ 200 High Purity Bentonite, Industrial Grade Suspengel products are manufactured from the highest quality Western Bentonite reserves. Suspengel products are easy to disperse thixotropes with excellent suspension properties. Strict process co.. |
|||
Bulk Density | 1.15 g/cc | 0.0417 lb/in³ | |
CIMBAR Suspengel™ 200 Plus High Purity Bentonite, Industrial Grade Suspengel products are manufactured from the highest quality Western Bentonite reserves. Suspengel products are easy to disperse thixotropes with excellent suspension properties. Strict process co.. |