Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.810 g/cc | 0.0293 lb/in³ | Poured; ASTM D1895 |
Eastman BD445 PET
(discontinued **) Voridian Polymer BD445 is primarily targeted for the soft drink and water markets, it is also suitable for use in other beverage containers as well as food and on-food-related applications. This pol.. |
|||
Bulk Density | 0.810 g/cc | 0.0293 lb/in³ | Poured (Mexico Produced); ASTM D1895 |
Eastman CB12 PET
(discontinued **) Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good ov.. |
|||
Bulk Density | 0.810 - 0.890 g/cc | 0.0293 - 0.0322 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 125 R Refractory Insulating Castable Description: Golite 125 R has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products. Also availa.. |
|||
Bulk Density | 0.810 g/cc | 0.0293 lb/in³ | ASTM D1895 |
Plenco 6343 Phenolic, Granular, Transfer Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Bulk Density | 0.810 g/cc | 0.0293 lb/in³ | |
DuPont™ Nomex® N196 Paper, 5 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Bulk Density | 0.810 g/cc | 0.0293 lb/in³ | ASTM D1895 |
Plenco 1581 Polyester, Briquette, Transfer Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |