Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.801 g/cc | 0.0289 lb/in³ | Poured; ASTM D1895 |
Eastman Aqua 18696 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186.. |
|||
Bulk Density | 0.801 - 0.897 g/cc | 0.0289 - 0.0324 lb/in³ | Loose |
KaMin KaMin® HG Kaolin Clay - Waterwashed KaMin® HG is an economical, general purpose, water-washed kaolin with fine particle size and intermediate brightness. It is suitable for water borne paint, ink and adhesive applications.Industry:.. |
|||
Bulk Density | 0.801 - 0.897 g/cc | 0.0289 - 0.0324 lb/in³ | Loose |
KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness KaMin® HG90 is a high brightness, ultra-fine particle size, platy kaolin with moderate water demand providing good tinting strength, Ti02 extension and gloss in water based paints. KaMin® HG90.. |
|||
Bulk Density | 0.801 - 0.897 g/cc | 0.0289 - 0.0324 lb/in³ | Loose |
KaMin KaMin® Tek 2001 Clay The uniform, narrow particle size distribution and excellent color makes Kamin® TEK 2001 the preferred extender for gloss latex paints where optimum TiO2 spacing is desired without adverse effect.. |
|||
Bulk Density | >= 0.801 g/cc | >= 0.0289 lb/in³ | |
Indorama Auriga Polymers Polyclear™ Perserve 2201 PET Resin Description: Polyclear® Preserve PET 2201 is designed to offer exceptional performance in hot-fill and pasteurized container applications. It has a nominal intrinsic viscosity of 0.82 dl/g. Packa.. |
|||
Bulk Density | 0.801 - 0.897 g/cc | 0.0289 - 0.0324 lb/in³ | Loose |
KaMin Polyfil® HG Kaolin Clay - Waterwashed Polyfil® HG is an ultra-fine particle size, moderate brightness water washed kaolin clay. It offers acid resistance, barrier properties, reinforcement, neutral ph, and extremely low crystalline .. |
|||
Bulk Density | 0.801 - 0.897 g/cc | 0.0289 - 0.0324 lb/in³ | Loose |
KaMin Polyfil® HG90 Kaolin Clay - Waterwashed High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R.. |
|||
Bulk Density | 0.801 g/cc | 0.0289 lb/in³ | Dry |
Skamol Group Moler ROTOL Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Bulk Density | 0.801 g/cc | 0.0289 lb/in³ | Defined by casting method, +/- 50kg (110 lbs) |
Skamol Group SKAMOCAST 112-80 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Bulk Density | 0.801 g/cc | 0.0289 lb/in³ | Dry |
Skamol Group SKAMOLEX V-1100 (800) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Bulk Density | 0.801 g/cc | 0.0289 lb/in³ | Loose |
Excalibar ExCal® 400 Calcium Carbonate CaCO3 Powder ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other appli.. |
|||
Bulk Density | 0.801 g/cc | 0.0289 lb/in³ | Dow Method |
Dow XU 32019.10 Barrier Polymer Excellent oxygen and water vapor barrier Information provided by Dow |
|||
Bulk Density | 0.801 g/cc | 0.0289 lb/in³ | Dow Method |