Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Loose |
Nyco NYAD G® WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Tapped |
Nyco NYAD® 1250 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Tapped |
Nyco NYAD® G Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Tapped |
Nyco NYGLOS® 20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 713-40 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 725-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
Invista 2201 PET Copolymer Packaging Resin
(discontinued **) Carboxyl end groups: |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-07C PET Bottle Grade A co-polymer used mostly for containers. |
|||
Bulk Density | 0.800 - 1.10 g/cc | 0.0289 - 0.0397 lb/in³ | |
Magyar Aluminum ALO-DFC Alumina Alumina for Polishing |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Lanxess Pocan® BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Lanxess Pocan® ECO T 3220 000000 PBT + PET, 20% Glass Fiber PBT + PET, 20% glass fibers, injection molding, improved surface finish, contains 28% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Lanxess Pocan® ECO T 3230 000000 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, contains 30% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Lanxess Pocan® T 7391 POS151 900044 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load UV stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Lanxess Pocan® B 1701 000000 PBT PBT, non-reinforced, extrusion, food contactInformation provided by LANXESS. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America E 2748-9641D Short Glass Fiber Reinforced Epoxy E 2748-9641D is a mineral and short fiberglass filled epoxy molding compound.Information provided by Sumitomo Bak North America, Inc. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America E 8354A-2 Short Glass Fiber Reinforced Epoxy E 8354A-2 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Powder Density; ASTM D1895 |
Sumitomo Bakelite North America E 8940SG Electrical Encapsulation Grade Epoxy Mineral reinforced epoxy molding compound formulated for the encapsulation of electronic devices requiring high quality, exceptional reliability, and outstanding moldability. USES: Passive electron.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Compression Grade Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 2061B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 2061B-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by S.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
Solvay SUPRAGIL® RM/210 EI Polynaphthalenmethan-Sulphonate, Sodium Salt Description: Dispersing, non foaming agent.Identification: POLYNAPHTHALENMETHAN-SULPHONATE, SODIUM SALTCAS: 9084 – 06 – 4Solubility: Soluble in water. Insoluble in polar and aromatic solve.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Size E (tapped) |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Poured; ASTM D1895 |
Eastman Aqua PJ003 PET Voridian Aqua PET PJ003 is a condensation polymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. This product is specifically designed f.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
DuPont™ Nomex® 410 Paper, 3 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
BASF Sicopal® Yellow K 1160 FG Color Additive Chemical Structure: Bismut-vanadium oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA and PARecommendations for food applications: BgVV, FrancePhysical form.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
BASF Sicotan® Yellow K 2111 FG Color Additive Chemical Structure: Cr/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
Addcomp ADD-VANCE® BA 401 Blowing agent Fields of application: Foamed products of Polyolefin and other polymers.Examples: Extruded sheets and foams in general as well as injection molded parts that require a foamed core.Mode of action and.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac FM 4005 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is compliant with the specificat.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Bulk Density measured via tamp density method after 1500 tamps |
Potters Industries A-Series Z-CEL® 8054 White Synthetic Sodium Aluminosilicate Microsphere Fine particle white spheres developed as filler for paints, coatings and films.Information provided by Potters Industries. |