Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Nabaltec ACTILOX® B20 AlO(OH) Boehmite Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature stabilitySynergistic effects with other flame retardantsHigh acid resistance.. |
|||
Bulk Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | |
Nabaltec NABALOX® NO 113 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
NanoScale NanoActive® Titanium Dioxide NanoActive TiO2 is produced using proprietary processes to obtain high specific surface area (over 500 m²/g), high porosity, weakly aggregated, amorphous material possessing adsorption capacity and.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895B |
SABIC PS 126 General Purpose Polystyrene for Injection Molding Product Description: General purpose Polystyrene PS 125 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and hi.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895B |
SABIC PS 155 General Purpose Polystyrene for Foam Extrusion Product Description: General purpose Polystyrene PS 155 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and go.. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | |
Raschig Group PiMC 1221 High gloss PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895B |
SABIC PS 330 High Impact Polystyrene for Sheet Extrusion Product Description: High Impact Polystyrene PS 330 is manufactured by continuous mass polymerization of styrene monomer. An elastomer is incorporated during polymerization to achieve impact resis.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 60 |
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 60 |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 60 |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 60 |
Lanxess Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Solvay REPEL-O-TEX® SRP-6 Polyethylene Glycol Polyester Description: Soil Release Polymer offering protection against the adhesion of greasy soils between two wash cycles. 100% active material in powder form.Chemical Name: POLYETHYLENE GLYCOL POLYESTERCA.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plenco 2369 Phenolic, Granular, Transfer Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Plenco 7100 Phenolic, Nodular, Injection Molded PLENCO 07100 is an organic fiber reinforced phenolic molding compound, with improved mechanical strength properties and an industrial finish. 07100 is densified for easy handling and good pourabilit.. |
|||
Bulk Density | 0.600 - 0.750 g/cc | 0.0217 - 0.0271 lb/in³ | Powder Density; ISO 60 |
Vyncolit 4221 XB Novolac Phenolic Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | Powder Density; ISO 60 |
Vyncolit X7010 Novolac Phenolic Glass fiber reinforced molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 1183 |
Polyram RamClean™ 101 Purging Agent Purging agent for injection molding machines.Information provided by Polyram. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 186 PVC PVC Copolymer Suspension Resin F-186 is a medium molecular vinyl chloride/vinyl acetate copolymer suspension resin. This resin is primarily used in the calendaring and extrusion of rigid film F-186 .. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 265 PVC PVC Copolymer Blending Resin F-265 is a fine particle size polyvinyl chloride vinyl acetate copolymer plastisol blending resin. The product has been designed for use in application where rapid gelat.. |
|||
Bulk Density | 0.600 - 0.750 g/cc | 0.0217 - 0.0271 lb/in³ | Powder Density; ISO 60 |
Vyncolit 2950 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | ISO 60 |
Vyncolit Neopreg Kinel® SK4503 S5 Aramid Reinforced Molding Compound Long aramid fiber reinforced BMI molding compound suited for very demanding tribologic applications under medium to poor lubricated conditions, high temperatures & PV levelsInformation provided by S.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Axion Polymers Axplas® PS04 0000 Mixed Polystyrene Granules with FR The PS04 series of clean, mixed polystyrene granular chips offers a low-cost option for manufacturers to add post-consumer, engineering polymers to a wide range of products. The polymer mix includes.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
Azoty Tarnow™ TARFLEN SG-1 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Styropor® F 315-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkageApplicati.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Styropor® F 395 -N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Styropor® P 326 M Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded parts with very good mechanical .. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Styropor® F 495-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Bulk Density | 0.600 g/cc | 0.0217 lb/in³ | |
BASF Styropor® P 426 Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts.Information pr.. |
|||
Bulk Density | 0.600 - 0.900 g/cc | 0.0217 - 0.0325 lb/in³ | |
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |