Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade
(discontinued **) ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H4262 High Density Polyethylene, Injection Molding Grade
(discontinued **) ApplicationsAlathon H4262 is a high-flow resin that exhibits very good cold temperature impact performance, optimum processing and thermal stability, with good color and organoleptic properties. Typ.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade ALATHON H4250 is a high-flow “freezer†grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H4620 High Density Polyethylene, Injection Molding Grade Alathon H4620 is a medium-flow resin that exhibits good cold temperature impact performance, enhanced processing and thermal stability. Typical applications are thinner-walled parts that require che.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, c.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade ALATHON M5352 is a high density copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good proces.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® M5372 High Density Polyethylene ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. .. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include case.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H5112 High Density Polyethylene, Injection Molding Grade ALATHON H5112 is a medium-molecular-weight-distribution resin with balanced impact/ESCR and high flow characteristics. Typical applications include housewares, food containers, pail handles and toys.. |
|||
Bulk Density | 0.593 g/cc | 0.0214 lb/in³ | Tapped |
CIMBAR EliteTalc® 23 Cosmetic Talc Cimbar performance Minerals MV, LLC Talc U.S.P. Cosmetic talcs are designed specifically for cosmetic formulations. Talc is commonly used in cosmetics for its ability to bind to oils, create a mois.. |