Physical Properties Metric English Comments
Bulk Density 0.570 g/cc
0.0206 lb/in³
Tapped
Nyco NYGLOS® 12 Wollastonite
High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv..
Bulk Density 0.570 g/cc
0.0206 lb/in³
M Chemical GUARD DOGâ„¢ UV622 HALS Light Stabilizer
GUARD DOGâ„¢ UV662 is a solid, polymeric type, free radical scavenger hindered amine light stabilizer that is used to protect a wide range of polymers against degradation caused by exposure to UV..
Bulk Density 0.570 - 0.630 g/cc
0.0206 - 0.0228 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 1.0.6. Mix Refractory Insulating Castable
Description: This castable is composed of a high quality alumina cement and vermiculite and is applied as a backlining. Special additives are responsible for the low shrinkage. This castable can be ..
Bulk Density 0.570 g/cc
0.0206 lb/in³
DIN 53466
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Bulk Density 0.570 g/cc
0.0206 lb/in³
DIN 53466
Silon Taborex TA 1133 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1133 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Bulk Density 0.570 g/cc
0.0206 lb/in³
ASTM D1895
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755..
Bulk Density 0.570 g/cc
0.0206 lb/in³
ISO 60
Vyncolit Vyntec® CF8050 Carbon Fiber Reinforced Phenolic
VYNTEC CF8030 is a carbon fiber reinforced phenolic moldable composite with excellent tribological properties. It has high mechanical strength combined with low density.Information provided by Sumit..
Bulk Density 0.570 g/cc
0.0206 lb/in³
ISO 60
Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic
VYNTEC CF8050 is a carbon fiber reinforced phenolic moldable composite with good tribological and superior mechanical properties combined with low density. Very good chemical resistance in several o..
Bulk Density 0.570 g/cc
0.0206 lb/in³
ASTM D1895
Formosa Plastics Formolon® 260 PVC
PVC Homopolymer Blending Resin F-260 is a fine particle size PVC homopolymer plastisol blending resin. It combines excellent fusion characteristics, low plastisol viscosities as well as lot to lot u..
Bulk Density 0.570 g/cc
0.0206 lb/in³
ASTM D1895
Formosa Plastics Formolon® 608 PVC
PVC Homopolymer General Purpose Grade Resin F608 is a low molecular weight PVC homopolymer of particular interest in rigid applications and has established a deserved reputation for low gels and exc..
Bulk Density 0.570 g/cc
0.0206 lb/in³
ASTM D1895
Formosa Plastics Formolon® 622 PVC
Homopolymer Pipe Grade Resin F622 is a medium-low molecular weight PVC homopolymer designed primarily for rigid extrusion applications. This product has excellent dry flow characteristics, making i..
Bulk Density 0.570 g/cc
0.0206 lb/in³
Daikin POLYFLON FA-500 MPA, White Powder
White powder.Major Uses: Addition of a minute amount of resins produces excellent anti-dripping properties. Good dispersion into resins enables production of moldings with better appearance than wi..
Bulk Density 0.570 g/cc
0.0206 lb/in³
ASTM D1895
Plenco 7307 Phenolic, Granular, Transfer Molded
PLENCO 07307 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties. Type ASTM 5948 CFG, and UL recognized under component file E40654. 07307 is a..
Bulk Density 0.570 g/cc
0.0206 lb/in³
ASTM D1895
Plenco 7321 Phenolic, Nodular, Injection Molded
PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon..
Copyright © lookpolymers.com All Rights Reserved