Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | Tapped |
Nyco NYGLOS® M3 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | |
SGL Carbon Group CF 1135 Carbon Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | DIN 53466 |
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | ASTM D1895 |
Plenco 7591 Phenolic, Briquette, Injection Molded PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | ASTM D1895 |
Westlake 1230P PVC Westlake PVC 1230P resin is a general purpose, medium molecular weight homopolymer designed primarily for the extrusion of rigid PVC products.Information provided by Westlake Chemical Corporation |
|||
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | ASTM D1895 |
Westlake 1230S PVC Westlake PVC 1230S resin is a medium molecular weight homopolymer designed primarily for the extrusion of rigid products.Information provided by Westlake Chemical Corporation |
|||
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 113 PVC PVC Copolymer Suspension Resin F-113 has been developed primarily to meet the processing requirements of the vinyl composition tile (VCT) manufacturers. In addition to vinyl floor tile industry, F-1.. |
|||
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 614 PVC Homopolymer - General Purpose Grade Resin F614 is a medium-low molecular weight PVC homopolymer of particular interest in rigid applications and has established a deserved reputation for low gels an.. |
|||
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 622E PVC Rigid Extrusion Resin F622E is a medium-low molecular weight PVC designed primarily for rigid extrusion applications. This product has excellent dry flow characteristics, making it desirable for dry.. |
|||
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 622R PVC Homopolymer General Purpose Grade Resin F622R is a medium-low molecular weight PVC homopolymer of interest in both rigid and flexible applications and has established a deserved reputation for low .. |
|||
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | ASTM D1895 |
Equate EGDA-6888 HDPE Film Extrusion Resin EGDA-6888 is a high molecular weight, high density polyethylene copolymer that has been designed specifically for tubular film extrusion. Its broad molecular weight distribution and density have bee.. |
|||
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | |
Asahi Glass Fluon® L170J PTFE Lubricant Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As.. |
|||
Bulk Density | 0.560 g/cc | 0.0202 lb/in³ | |
Asahi Glass Fluon® L172J PTFE Lubricant Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As.. |