Polymer Property : Bulk Density = 0.545 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.545 g/cc
0.0197 lb/in³
Dry
Skamol Group ISOPERLOR 550P Perlite Insulating Brick & Block
ISOPERLOR perlite insulating bricks & blocks have the following characteristics: Max. service temperature 900°C (1652°F)Back-up insulation onlyExcellent insulating propertiesVery lightweight a..
Bulk Density 0.545 g/cc
0.0197 lb/in³
As Supplied
Skamol Group Moler BB-Filler Aggregate Insulation
SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre..
Bulk Density 0.545 g/cc
0.0197 lb/in³
Dry
Skamol Group Moler HIPOR Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Bulk Density 0.545 g/cc
0.0197 lb/in³
As Supplied
Skamol Group SKAMOCAST 112-80 Insulating Castable
SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f..
Bulk Density 0.545 g/cc
0.0197 lb/in³
Loose
CIMBAR RiverCal™ 8103 & 8103C Calcium Carbonate (CaCO3)
RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications..