Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.330 g/cc | 0.0119 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® N 347 ASTM Carbon Black Standard grade of furnace black in accordance with the requirements of ASTM D 1765Hard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.330 g/cc | 0.0119 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons ECORAX® S 247 Carbon Black Specialty black for tire treads and bodies that provide reduced rolling resistanceInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.330 - 0.390 g/cc | 0.0119 - 0.0141 lb/in³ | ASTM D1895 |
Polimeros Mexicanos Rotofoam® Plus 93050 Medium Density Polyethylene, Foam Grade Hexene Copolymer Linear Medium Density Polyethylene for foaming applications. It is formulated for inner layers with excellent foam cell structure and smooth surface finish and uniform closed cells... |
|||
Bulk Density | 0.330 - 0.390 g/cc | 0.0119 - 0.0141 lb/in³ | ASTM D1895 |
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized.Recommended for general purpose applications. Frequently used for water tanks (less tha.. |
|||
Bulk Density | 0.330 - 0.390 g/cc | 0.0119 - 0.0141 lb/in³ | ASTM D1895 |
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene MDPE Copolymer with UV8 stabilizer in natural and colors.Recommended for rotomolding. Used for manufacture of water tanks > 2000 liters, cisterns, farm tanks, or tanks to contain strong acids and b.. |
|||
Bulk Density | 0.330 - 0.390 g/cc | 0.0119 - 0.0141 lb/in³ | ASTM D1895 |
Polimeros Mexicanos Rotolene® Black Plus Polyethylene Polyethylene compound specially formulated for rotational molding applications requiring good mechanical properties and good mold release properties. Rotational molded parts have smooth surface and .. |
|||
Bulk Density | 0.330 - 0.390 g/cc | 0.0119 - 0.0141 lb/in³ | ASTM D1895-96 |
Polimeros Mexicanos Rotolene® Black Plus Ultra Polyethylene Linear copolymer Medium Density Polyethylene which is fully UV8 stabilized. Available as black powder.Applications: Polyethylene compound specially formulated for rotational molding applications req.. |
|||
Bulk Density | 0.330 - 0.390 g/cc | 0.0119 - 0.0141 lb/in³ | ASTM D1895 |
Polimeros Mexicanos Rotolene® Diesel Tank Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized.High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks a.. |
|||
Bulk Density | 0.330 g/cc | 0.0119 lb/in³ | ISO 60 |
SABIC PVC 741E Emulsion Polyvinyl Chloride for Paste Preparation Product Description: PVC 741E is a fine particle, high molecular weight PVC homopolymer, made by emulsion polymerization. It is designed for the manufacture of plastisols exhibiting low viscositie.. |
|||
Bulk Density | 0.330 g/cc | 0.0119 lb/in³ | |
Solvay RHODORSIL® EP 6703 Surfactant Description: Antifoam for dry and liquid formulationsIdentification: ABSORBED POLYDIMETHYLSILOXANEAvailable in: Asia Pacific, Europe, Latin America and North America.Solubility: Dispersible in water.. |
|||
Bulk Density | 0.330 g/cc | 0.0119 lb/in³ | Scott |
TIMCAL TIMREX® T15-75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.330 g/cc | 0.0119 lb/in³ | |
BASF Heligoen® Blue K 6911 D Color Additive Chemical Structure: Cu-phthalocyanine alpha stabApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PA, PETP, CA/CAB, and UPRecommendations for food applicat.. |
|||
Bulk Density | 0.330 g/cc | 0.0119 lb/in³ | |
Asahi Glass Fluon® G163 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |