Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0900 g/cc | 0.00325 lb/in³ | Scott, Typical |
TIMCAL TIMREX® C-LUB 304 Primary Synthetic Graphite Information provided by TIMCAL |
|||
Bulk Density | 0.0900 g/cc | 0.00325 lb/in³ | Scott |
TIMCAL TIMREX® F10 Primary Synthetic P/M Special-Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.0900 g/cc | 0.00325 lb/in³ | Scott, Typical |
TIMCAL TIMREX® KS10 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production.. |
|||
Bulk Density | 0.0900 g/cc | 0.00325 lb/in³ | Scott |
TIMCAL TIMREX® MB15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.0900 g/cc | 0.00325 lb/in³ | Scott |
TIMCAL TIMREX® MK25 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.0900 g/cc | 0.00325 lb/in³ | Scott |
TIMCAL TIMREX® SFG15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |