Polymer Property : Bulk Density = 0.0700 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.0700 g/cc
0.00253 lb/in³
Scott, Typical
TIMCAL TIMREX® C-LUB 302 Primary Synthetic Graphite
Information provided by TIMCAL
Bulk Density 0.0700 g/cc
0.00253 lb/in³
Scott, Typical
TIMCAL TIMREX® KS6 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production..
Bulk Density 0.0700 g/cc
0.00253 lb/in³
Scott
TIMCAL TIMREX® LSG6 Natural Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Bulk Density 0.0700 g/cc
0.00253 lb/in³
Scott
TIMCAL TIMREX® MK15 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Bulk Density 0.0700 g/cc
0.00253 lb/in³
Scott
TIMCAL TIMREX® PG25 Natural P/M Special-Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Bulk Density 0.0700 g/cc
0.00253 lb/in³
Scott
TIMCAL TIMREX® SFG10 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Bulk Density 0.0700 g/cc
0.00253 lb/in³
Scott
TIMCAL TIMREX® SFG6 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Bulk Density 0.0700 g/cc
0.00253 lb/in³
Scott
TIMCAL TIMREX® KS4 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..