Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0333 g/cc | 0.00120 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN LSP-30EB Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0333 g/cc | 0.00120 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN OP-30DB Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0333 g/cc | 0.00120 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN OP-30E Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0333 g/cc | 0.00120 lb/in³ | After expansion |
Sekisui PIOCELAN OP-30EU (Low VOC, Low odor) Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0333 g/cc | 0.00120 lb/in³ | After expansion |
Sekisui PIOCELAN OP-E30ENS (Antistatic) Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0333 g/cc | 0.00120 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN TOPF-30DB Flame Retardant Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |